Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Goodfellow
Trade Name Awa®, Nickeloid®, Simlet®, Spedex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Awa®, Nickeloid®, Simlet®, Spedex® Nickel Silver.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good machinability, excellent cold working and welding characteristics. Poor hot forming. Uses include rivets, screws, zippers, optical parts and costume jewelry.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 8.72 g/cc
0.315 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 75 - 190
75 - 190
Tensile Strength at Break 400 - 700 MPa
58000 - 102000 psi
Elongation at Break <= 45 %
<= 45 %
Tensile Modulus 120 - 135 GPa
17400 - 19600 ksi
Shear Strength 290 - 400 MPa
42100 - 58000 psi
Izod Impact, Unnotched 1.10 - 1.30 J/cm
2.06 - 2.44 ft-lb/in
Notch Status Unknown
Thermal Properties Metric English Comments
CTE, linear 16.0 - 17.1 µm/m-°C

@Temperature 25.0 - 300 °C
8.89 - 9.50 µin/in-°F

@Temperature 77.0 - 572 °F
Thermal Conductivity 28.0 W/m-K
194 BTU-in/hr-ft²-°F
Melting Point 1060 - 1110 °C
1940 - 2030 °F
Solidus 1060 °C
1940 °F
Liquidus 1110 °C
2030 °F
Component Elements Properties Metric English Comments
Copper, Cu 62 %
62 %
Nickel, Ni 18 %
18 %
Zinc, Zn 20 %
20 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000290 ohm-cm
0.0000290 ohm-cm
Temperature Coefficient of 0.0003/K