Arlon AD255A Glass, PTFE and Micro-Dispersed Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon AD255A Glass, PTFE and Micro-Dispersed Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lower Loss and Improved Performance over Traditional AD Series.Information provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Water Absorption 0.040 %
0.040 %
Mechanical Properties Metric English Comments
Peel Strength 2.10 kN/m
12.0 pli
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C
8.89 µin/in-°F
x direction
16.0 µm/m-°C
8.89 µin/in-°F
y direction
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
z direction
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 2.55

@Frequency 1.00e+10 Hz
2.55

@Frequency 1.00e+10 Hz
2.55

@Thickness 0.762 mm
2.55

@Thickness 0.0300 in
2.55

@Thickness 1.57 mm
2.55

@Thickness 0.0620 in
Dissipation Factor 0.0015

@Frequency 1.00e+10 Hz
0.0015

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -138