Material Notes:
Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX
Physical Properties Metric English Comments
Density 8.65 g/cc
0.313 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers >= 175
>= 175
Tensile Strength, Ultimate 570 - 780 MPa
82700 - 113000 psi
Tensile Strength, Yield >= 55.0 MPa

@Strain 0.200 %
>= 7980 psi

@Strain 0.200 %
Elongation at Break 3.0 %
3.0 %
100 A
Modulus of Elasticity 130 GPa
18900 ksi
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 0.000 - 100 °C
8.89 µin/in-°F

@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.410 J/g-°C
0.0980 BTU/lb-°F
Thermal Conductivity 33.0 W/m-K
229 BTU-in/hr-ft²-°F
Melting Point 1020 °C
1870 °F
Component Elements Properties Metric English Comments
Copper, Cu 63 %
63 %
Lead, Pb <= 1.0 %
<= 1.0 %
Nickel, Ni 13 %
13 %
Zinc, Zn <= 23 %
<= 23 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000230 ohm-cm
0.0000230 ohm-cm
Descriptive Properties Value Comments
Color Ivory