Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 - 110 °C | 215 - 230 °F | Average value: 106 °C Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® FR134G10 ABS, 10% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | unannealed, .125in; ASTM D648 |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF/M30 CC BK 30% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 30% Filler by WeightFeatures: Chemically Coupled and CopolymerAppearance: BlackInformation provided by TP Composites, In.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM HO TL20 BN042 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerAppearance: Brown, Natural Color and RedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Techmer ES Plaslube® AC-80/TF/15 Acetal (Copolymer), 15% PTFE Plaslube polytetrafluoroethylene (PTFE) lubricated acetal copolymer grades offer additional wear and friction performance over neat acetal. Typical applications include bearings, slides and small g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® ABS E AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM Test |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C @Thickness 3.17 mm |
215 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A220G ABS Molding Resin, 20% Glass Fiber Reinforced Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® APC300 ABS Polycarbonate Alloy, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Westlake Plastics Absylux® CN-F Acrylonitrile-Butadiene-Styrene (conductive) Non-sloughing, carbon-fiber-filled material with high strength and stiffness; easily machined.Information provided by Westlake Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | 0.125 in bar Annealed 4 hours at 80°C; ASTM D648 |
Diamond Polymers ABS 3501 GF-20 Description: Reinforced Grade, 20%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Chase Plastics CP Pryme® PCA300 General Purpose Polycarbonate/ABS Alloy (Utility Grade) Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |