Westlake Plastics Absylux® CN-F Acrylonitrile-Butadiene-Styrene (conductive)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
Manufacturer Westlake Plastics
Trade Name Absylux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Absylux® CN-F Acrylonitrile-Butadiene-Styrene (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-sloughing, carbon-fiber-filled material with high strength and stiffness; easily machined.Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Water Absorption 0.26 %
0.26 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 118.9 MPa
17250 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 162 MPa
23500 psi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm - 1e+05
100 ohm-cm - 1e+05
Dry; ASTM D257
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
Dry; ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
15% RH; MIL-B-81705-B