Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 102 - 110 °C | 215 - 230 °F | Average value: 106 °C Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 - 110 °C | 125 - 230 °F | Average value: 74.1 °C Grade Count:52 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 104 - 110 °C | 219 - 230 °F | ASTM D648 |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 - 110 °C | 176 - 230 °F | GB/1634 |
Zhejiang Juner PC/PBT Alloy Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 - 110 °C | 176 - 230 °F | GB/1634 |
Zhejiang Juner PC/PET Alloy Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 47.8 - 110 °C | 118 - 230 °F | Average value: 60.4 °C Grade Count:34 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |