Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® APC300 ABS Polycarbonate Alloy, Recycled Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® APC300 ABS Polycarbonate Alloy, Recycled Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Recycled contentForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Yield Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 3.74 J/cm
7.00 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C
215 °F
Unannealed; ASTM D648
Users viewing this material also viewed the following: