Material Notes:
Borstar® HE3410 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an optimized stabilization system. Borstar® HE3410 is classified as an MRS 8.0 material (PE80). Applications: Borstar® HE3410 is recommended for pressure and non pressure pipe systems in the application fields of sewerage waste water piping systems, landfill drainage pipes, sheets, casings and ducting pipes as well as guard tubes.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Oxidative Induction Time (OIT) >= 15 min

@Temperature 210 °C
>= 15 min

@Temperature 410 °F
EN 728
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Charpy Impact, Notched 1.40 J/cm²

@Temperature 0.000 °C
6.66 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ISO 75-2
Vicat Softening Point 72.0 °C

@Load 5.10 kg
162 °F

@Load 11.2 lb
B50; ISO 306
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Processing Properties Metric English Comments
Middle Barrel Temperature 180 - 210 °C
356 - 410 °F
cylinder
Die Temperature 200 - 210 °C
392 - 410 °F
Melt Temperature 200 - 210 °C
392 - 410 °F
Head Temperature 200 - 210 °C
392 - 410 °F