Thermal Properties Metric English Comments
Brittleness Temperature -70.0 - -35.0 °C
-94.0 - -31.0 °F
Average value: -67.0 °C Grade Count:25
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a..