Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.05 - 1.53 g/cc
0.0379 - 0.0553 lb/in³
Average value: 1.14 g/cc Grade Count:156
Loss On Ignition 28.0 - 32.0 %
28.0 - 32.0 %
Average value: 30.0 % Grade Count:5
Water Vapor Transmission 3000 - 3000 g/m²/day

@Temperature 38.0 - 38.0 °C
193 - 193 g/100 in²/day

@Temperature 100 - 100 °F
Average value: 3000 g/m²/day Grade Count:1
Viscosity 72000 - 72000 cP

@Temperature 204 - 204 °C
72000 - 72000 cP

@Temperature 399 - 399 °F
Average value: 72000 cP Grade Count:1
Maximum Moisture Content 0.0200 - 0.0500
0.0200 - 0.0500
Average value: 0.0223 Grade Count:26
Linear Mold Shrinkage 0.00110 - 0.0150 cm/cm
0.00110 - 0.0150 in/in
Average value: 0.00698 cm/cm Grade Count:50
Linear Mold Shrinkage, Transverse -0.00300 - 0.00900 cm/cm
-0.00300 - 0.00900 in/in
Average value: 0.00457 cm/cm Grade Count:22
Melt Flow 1.20 - 150 g/10 min
1.20 - 150 g/10 min
Average value: 39.0 g/10 min Grade Count:49
Mechanical Properties Metric English Comments
Hardness, Shore A 52.0 - 98.0
52.0 - 98.0
Average value: 85.3 Grade Count:134
Hardness, Shore D 22.0 - 95.0
22.0 - 95.0
Average value: 49.1 Grade Count:68
Tensile Strength, Ultimate 2.60 - 65.5 MPa
377 - 9500 psi
Average value: 34.8 MPa Grade Count:158
28.42 - 60.0 MPa

@Temperature 70.0 - 100 °C
4122 - 8700 psi

@Temperature 158 - 212 °F
Average value: 46.5 MPa Grade Count:6
28.42 - 60.0 MPa

@Time 0.000 - 4.84e+6 sec
4122 - 8700 psi

@Time 0.000 - 1340 hour
Average value: 46.5 MPa Grade Count:6
Tensile Strength, Yield 1.70 - 44.1 MPa
247 - 6400 psi
Average value: 11.3 MPa Grade Count:147
Elongation at Break 30.0 - 1000 %
30.0 - 1000 %
Average value: 582 % Grade Count:161
Modulus of Elasticity 0.0110 - 2.07 GPa
1.60 - 300 ksi
Average value: 0.243 GPa Grade Count:12
Flexural Modulus 0.0171 - 1.31 GPa
2.48 - 190 ksi
Average value: 0.248 GPa Grade Count:30
Resilience 35.0 - 52.0
35.0 - 52.0
Average value: 42.7 Grade Count:7
Rebound 25.0 - 72.0 %
25.0 - 72.0 %
Average value: 41.8 % Grade Count:23
Shear Modulus 0.00840 - 0.150 GPa
1.22 - 21.8 ksi
Average value: 0.0519 GPa Grade Count:4
0.0138 - 0.3656 GPa

@Temperature -50.0 - 0.000 °C
2.00 - 53.03 ksi

@Temperature -58.0 - 32.0 °F
Average value: 0.159 GPa Grade Count:1
Tear Strength 12.4 - 257 kN/m
71.0 - 1470 pli
Average value: 87.5 kN/m Grade Count:147
Graves Tear Strength 21.0 - 175 kN/m
120 - 1000 pli
Average value: 86.8 kN/m Grade Count:26
Taber Abrasion, mg/1000 Cycles 2.00 - 350
2.00 - 350
Average value: 46.0 Grade Count:71
Compression Set 16.0 - 92.0 %
16.0 - 92.0 %
Average value: 37.2 % Grade Count:76
33.0 - 82.0 %

@Temperature 70.0 - 70.0 °C
33.0 - 82.0 %

@Temperature 158 - 158 °F
Average value: 51.6 % Grade Count:11
28.0 - 82.0 %

@Temperature 70.0 - 70.0 °C
28.0 - 82.0 %

@Temperature 158 - 158 °F
Average value: 51.6 % Grade Count:39
28.0 - 82.0 %

@Time 79200 - 86400 sec
28.0 - 82.0 %

@Time 22.0 - 24.0 hour
Average value: 51.6 % Grade Count:39
Tensile Set 6.00 - 130 %
6.00 - 130 %
Average value: 47.8 % Grade Count:50
Thermal Properties Metric English Comments
CTE, linear 88.7 - 175 µm/m-°C
49.3 - 97.2 µin/in-°F
Average value: 153 µm/m-°C Grade Count:22
88.7 - 170 µm/m-°C

@Temperature -80.0 - -30.0 °C
49.3 - 94.4 µin/in-°F

@Temperature -112 - -22.0 °F
Average value: 137 µm/m-°C Grade Count:6
Melting Point 110 - 200 °C
230 - 392 °F
Average value: 151 °C Grade Count:29
Vicat Softening Point 56.0 - 145 °C
133 - 293 °F
Average value: 92.1 °C Grade Count:68
Brittleness Temperature -70.0 - -35.0 °C
-94.0 - -31.0 °F
Average value: -67.0 °C Grade Count:25
Glass Transition Temp, Tg -69.0 - -17.0 °C
-92.2 - 1.40 °F
Average value: -40.2 °C Grade Count:49
Clash Berg Stiffness Temperature -38.0 - 6.11 °C
-36.4 - 43.0 °F
Average value: -8.59 °C Grade Count:3
Flammability, UL94 V-2 - V-0
V-2 - V-0
Grade Count:9
Optical Properties Metric English Comments
Haze 1.00 - 23.0 %
1.00 - 23.0 %
Average value: 7.02 % Grade Count:5
Transmission, Visible 90.0 %
90.0 %
Average value: 90.0 % Grade Count:9
Electrical Properties Metric English Comments
Electrical Resistivity 2.70e+9 - 1.00e+12 ohm-cm
2.70e+9 - 1.00e+12 ohm-cm
Average value: 3.01e+11 ohm-cm Grade Count:4
Surface Resistance 1.50e+10 - 1.00e+12 ohm
1.50e+10 - 1.00e+12 ohm
Average value: 3.04e+11 ohm Grade Count:4
Dielectric Constant 4.60 - 8.00
4.60 - 8.00
Average value: 6.34 Grade Count:3
Dielectric Strength 39.0 - 49.0 kV/mm
991 - 1240 kV/in
Average value: 44.7 kV/mm Grade Count:3
Dissipation Factor 0.0250 - 0.121
0.0250 - 0.121
Average value: 0.0560 Grade Count:3
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:7
Processing Properties Metric English Comments
Processing Temperature 130 - 221 °C
266 - 430 °F
Average value: 188 °C Grade Count:17
Nozzle Temperature 170 - 227 °C
338 - 441 °F
Average value: 197 °C Grade Count:25
Adapter Temperature 175 - 216 °C
347 - 421 °F
Average value: 193 °C Grade Count:41
Die Temperature 175 - 216 °C
347 - 421 °F
Average value: 194 °C Grade Count:46
Melt Temperature 150 - 227 °C
302 - 441 °F
Average value: 191 °C Grade Count:79
Head Temperature 190 - 200 °C
374 - 392 °F
Average value: 195 °C Grade Count:4
Mold Temperature 15.0 - 95.6 °C
59.0 - 204 °F
Average value: 39.6 °C Grade Count:42
Drying Temperature 80.0 - 110 °C
176 - 230 °F
Average value: 98.2 °C Grade Count:50
Moisture Content 0.0100 - 0.100 %
0.0100 - 0.100 %
Average value: 0.0467 % Grade Count:3
Dew Point -40.0 - -17.8 °C
-40.0 - 0.000 °F
Average value: -37.7 °C Grade Count:28
Injection Pressure 4.96 - 7000 MPa
720 - 1.02e+6 psi
Average value: 854 MPa Grade Count:4