Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chengdu Polyster H605 Thermoplastic Polyether-ester Elastomer (TPEE)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyether Ester Elastomer
Manufacturer Chengdu Polyster Co.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chengdu Polyster H605 Thermoplastic Polyether-ester Elastomer (TPEE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent tear resistance. Molded and injected products for consumer use, such as airbag door covers, railway tie pads, seals, wires, cables and optical fiber.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Melt Flow 6.0 - 8.0 g/10 min
6.0 - 8.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ISO 868
Tensile Strength, Ultimate 35.0 MPa
5080 psi
ISO 527-1
Elongation at Break 500 %
500 %
ISO 527-1
Flexural Modulus 0.206 GPa
29.9 ksi
ISO 178
Tear Strength 153 kN/m
873 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
ISO 3146
Brittleness Temperature -70.0 °C
-94.0 °F
ISO 974