Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer NOVA Chemicals
Trade Name Sclair®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Sclair® 2714 HDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent processability for applications requiring good stiffness and toughness, good cold temperature impact properties.Applications: Food containers and lids, frozen food containers.Data provided by the manufacturer.
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
Density 0.951 g/cc
0.0344 lb/in³
ASTM D792
Melt Flow 51 g/10 min

@Load 2.16 kg,
Temperature 190 °C
51 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 36.0 cm
14.2 in
NOVA Snake Flow Test
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength, Yield 23.0 MPa
3340 psi
50 mm/min; ASTM D638
29.0 MPa
4210 psi
500 mm/min
Elongation at Break 15 %
15 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 119 °C
246 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D696
Processing Properties Metric English Comments
Melt Temperature 170 - 280 °C
338 - 536 °F
Users viewing this material also viewed the following: