Material Notes:
This product is intended for general purpose injection molding applications especially those requiring fast cycle time, improved color, enhanced processability, and excellent clarity.Information provided by Entec
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
ASTM D955
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus, 1% Secant 960 MPa
139000 psi
ASTM D790
Izod Impact, Notched 0.700 J/cm

@Thickness 3.17 mm
1.31 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
ASTM D648