Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem JV 060U HDPE Injection Molding Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem JV 060U HDPE Injection Molding Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Caps, crates for industrial, transportation or fishing uses, industrial pails, stands and pallets, refuse containers; bottle cases, safety helmets, cages for poultry transportation and sporting goods. Information provided by Braskem
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D1505
ESCR 100% Igepal® 2.5 hour

@Thickness 3.00 mm,
Temperature 23.0 °C
2.5 hour

@Thickness 0.118 in,
Temperature 73.4 °F
compression molded plaques; ASTM D1693B
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 71.0 °C
160 °F
ASTM D648
Vicat Softening Point 125 °C
257 °F
ASTM D1525