Engineered Polymer Solutions ABS 550

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Engineered Polymer Solutions
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Engineered Polymer Solutions ABS 550.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Medium Impact. Natural and colors available. Medium gloss. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792-91
Melt Flow 12 g/10 min

@Load 10.0 kg,
Temperature 220 °C
12 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
Flexural Modulus 2.38 GPa
345 ksi
ASTM D790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C
195 °F
ASTM D648