Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTRODAL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTRODAL C FG Polyoxymethylene, Food Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
POM C is a partially crystalline thermoplastic, which is characterized by its excellent machinability, dimensional stability, and chemical resistance.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Moisture Absorption 0.200 %

@Temperature 23.0 °C
0.200 %

@Temperature 73.4 °F
normal humidity; ISO 62
Water Absorption at Saturation 0.80 %

@Temperature 23.0 °C
0.80 %

@Temperature 73.4 °F
ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 84
84
test piece 10mm thick; ISO 2039-2
Ball Indentation Hardness 140 MPa
20300 psi
ISO 2039-1
Tensile Strength 63.0 MPa
9140 psi
5 mm/min; ISO 527-2
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ISO 527-2
Elongation at Break 31 %
31 %
ISO 527-2
Tensile Modulus 2.60 GPa
377 ksi
ISO 527-2
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Charpy Impact Unnotched 22.0 J/cm²
105 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 23.0 - 60.0 °C
61.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359
Thermal Conductivity 0.310 W/m-K
2.15 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 165 °C
329 °F
DSC, 10 K/m; ISO 3146
Maximum Service Temperature, Air 105 °C
221 °F
continuous
140 °C
284 °F
short term
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
ISO 75-2
Vicat Softening Point 150 °C
302 °F
VST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB

@Thickness 3.00 - 6.00 mm
HB

@Thickness 0.118 - 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency 100 Hz
3.8

@Frequency 100 Hz
IEC 60250
3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0030

@Frequency 100 Hz
0.0030

@Frequency 100 Hz
IEC 60250
0.0080

@Frequency 1.00e+6 Hz
0.0080

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Color Blue
Natural
Food Compliance BfR: Yes
Food Compliance FDA Yes