Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.90 µm/m-°C @Temperature 25.0 - 200 °C |
5.50 µin/in-°F @Temperature 77.0 - 392 °F |
|
Osprey Metals CE9 Al-Si Controlled Expansion Alloy Si-40%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 800 °C |
5.50 µin/in-°F @Temperature 68.0 - 1470 °F |
|
Misumi Alumina 99 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.50 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG34 Conversion Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include FG3, FG13 |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 300 °C |
5.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG7 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 300 °C |
5.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott WG280 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 300 °C |
5.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF11 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 300 °C |
5.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 300 °C |
5.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF8 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 300 °C |
5.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF57HT Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 500 °C |
5.50 µin/in-°F @Temperature 68.0 - 932 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 500 °C |
5.50 µin/in-°F @Temperature 68.0 - 932 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 500 °C |
5.50 µin/in-°F @Temperature 68.0 - 932 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 0.000 - 100 °C |
5.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 410 Chromium Steel Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 0.000 - 100 °C |
5.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature -6.00 - 100 °C |
5.50 µin/in-°F @Temperature 21.2 - 212 °F |
|
Crucible Steel 416R Chromium Stainless Steel Crucible 416R is a pre-hardened chromium stainless steel which is suitable for use in precision match-grade rifle barrels. It can be supplied in various hardness ranges according to the specific req.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 260 °C |
5.50 µin/in-°F @Temperature 68.0 - 500 °F |
|
Crucible Steel CPM® REX® 66 (HS) High Speed Steel CPM Rex 66 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed with a high vanadium content for excellent abrasion resistance, simila.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 260 °C |
5.50 µin/in-°F @Temperature 68.0 - 500 °F |
|
Crucible Steel CPM® Rex® T15(HS), AISI T15 High Speed Steel Rex® T15(HS) CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobal.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 100 °C |
5.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 20.0 - 100 °C |
5.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 0.000 - 100 °C |
5.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |
|||
CTE, linear | 9.90 µm/m-°C @Temperature 0.000 - 100 °C |
5.50 µin/in-°F @Temperature 32.0 - 212 °F |
|
AK Steel 410 Martensitic Stainless steel AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different.. |