Crucible Steel 416R Chromium Stainless Steel

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer Crucible Steel
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Crucible Steel 416R Chromium Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crucible 416R is a pre-hardened chromium stainless steel which is suitable for use in precision match-grade rifle barrels. It can be supplied in various hardness ranges according to the specific requirements ( HRC 24/28, 28/32, or 32/36). Crucible 416R was specifically designed by Crucible engineers in collaboration with barrel makers and rifle manufacturers to provide consistency, high quality and the following characteristics: Good machinability for gun drilling and reaming, plus excellent polishability for uniform lapping, necessary for bore accuracy. A homogeneous microstructure which responds to heat treat providing a uniform hardness along the length of the bar, necessary for accurate button rifling to precise groove dimensions. An optimum combination of high tensile strength along with adequate toughness to withstand the typical chamber pressures encountered during firing. Good corrosion resistance to inhibit rusting and which also helps to minimize fouling. Crucible 416R provides a durable finish which does not pit when properly maintained. Precision straightened and stress relieved bars, either mill length or multi length, ready to be cut to length and gun drilled. 100% ultrasonic testing for reliable barrels.Crucible 416R stainless steel is manufactured using very stringent controls from initial melting, through hot rolling, heat treating, cold finishing and final bar inspection. Barrels made from Crucible 416R are used at all levels of competition and in all conditions dry, damp or salty. Although all martensitic stainless steels have reduced ductility at very low temperatures, Crucible 416R can be safely used down to minus 40°F (-40°C).Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 170
170
Hardness, Rockwell C 28 - 36
28 - 36
Modulus of Elasticity 200 GPa
29000 ksi
Tension
Shear Modulus 72.3 GPa
10500 ksi
Thermal Properties Metric English Comments
CTE, linear 9.90 µm/m-°C

@Temperature -6.00 - 100 °C
5.50 µin/in-°F

@Temperature 21.2 - 212 °F
10.1 µm/m-°C

@Temperature 0.000 - 315 °C
5.61 µin/in-°F

@Temperature 32.0 - 599 °F
11.5 µm/m-°C

@Temperature 0.000 - 538 °C
6.39 µin/in-°F

@Temperature 32.0 - 1000 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F

@Temperature 32.0 - 212 °F
Thermal Conductivity 25.1 W/m-K

@Temperature 93.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 199 °F
28.5 W/m-K

@Temperature 538 °C
198 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.12 %
0.12 %
Chromium, Cr 12.5 %
12.5 %
Iron, Fe 86.05 %
86.05 %
As Remainder
Manganese, Mn 0.40 %
0.40 %
Molybdenum, Mo 0.40 %
0.40 %
Silicon, Si 0.40 %
0.40 %
Sulfur, S 0.13 %
0.13 %