Material Notes:
Si-40%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals.
Mechanical Properties Metric English Comments
Modulus of Elasticity 118 GPa
17100 ksi
Flexural Strength 140 MPa
20300 psi
Three Point Bend
Thermal Properties Metric English Comments
CTE, linear 8.30 µm/m-°C

@Temperature 25.0 - 100 °C
4.61 µin/in-°F

@Temperature 77.0 - 212 °F
9.90 µm/m-°C

@Temperature 25.0 - 200 °C
5.50 µin/in-°F

@Temperature 77.0 - 392 °F
10.1 µm/m-°C

@Temperature 25.0 - 500 °C
5.61 µin/in-°F

@Temperature 77.0 - 932 °F
10.5 µm/m-°C

@Temperature 25.0 - 300 °C
5.83 µin/in-°F

@Temperature 77.0 - 572 °F
Specific Heat Capacity 0.780 J/g-°C
0.186 BTU/lb-°F
Thermal Conductivity 108 W/m-K

@Temperature 200 °C
750 BTU-in/hr-ft²-°F

@Temperature 392 °F
129.4 W/m-K

@Temperature 25.0 °C
898.0 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
Component Elements Properties Metric English Comments
Aluminum, Al 40 %
40 %
Silicon, Si 60 %
60 %
Users viewing this material also viewed the following: