Schott BG7 Band Pass Filter

Category Ceramic , Glass , Filter , Optical
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott BG7 Band Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.61 g/cc
0.0943 lb/in³
Thermal Properties Metric English Comments
CTE, linear 8.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.72 µin/in-°F

@Temperature -22.0 - 158 °F
9.90 µm/m-°C

@Temperature 20.0 - 300 °C
5.50 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 468 °C
874 °F
Optical Properties Metric English Comments
Refractive Index 1.52

@Wavelength 587.6 nm
1.52

@Wavelength 587.6 nm
He
1.54

@Wavelength 404.7 nm
1.54

@Wavelength 404.7 nm
Hg
Transmission, Visible <= 1.0 %

@Wavelength 610 - 700 nm
<= 1.0 %

@Wavelength 610 - 700 nm
52 %

@Wavelength 400 nm
52 %

@Wavelength 400 nm
Internal transmittance of 56% at 400 nm
73 %

@Wavelength 480 nm
73 %

@Wavelength 480 nm
Internal transmittance of 79% at 400 nm
IR Transmittance 74 %

@Wavelength 2200 nm
74 %

@Wavelength 2200 nm
Internal transmittance of 80% at 2200 nm.
UV Transmittance <= 1.0 %

@Wavelength 200 - 330 nm
<= 1.0 %

@Wavelength 200 - 330 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 1
1
Stain Resistance Class, FR 0.0
0.0