Thermal Properties Metric English Comments
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 30.0 °C
4.06 µin/in-°F

@Temperature 68.0 - 86.0 °F
X-Direction
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite
AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements ..
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 500 °C
4.06 µin/in-°F

@Temperature 68.0 - 932 °F
Misumi Alumina 96 Aluminum Oxide, Al2O3
Information provided by MISUMI Corporation.
CTE, linear 7.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott BG42 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott NG5 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG1, NG9, NG10, NG11, NG 12
CTE, linear 7.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BALF5 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BASF64 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LASF41 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-PSK3 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-SK14 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-SK16 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott P-LASF47 Glass
Suitable for precision moldingInformation Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott NG3 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG1, NG4, NG5, NG9, NG10, NG11, NG 12
CTE, linear 7.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-KZFS4 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-LAF7 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 400 °C
4.06 µin/in-°F

@Temperature 68.0 - 752 °F
DIN EN 821-1
CeramTec B 601 Alumina, 98.5%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 600 °C
4.06 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C372
CeramTec Rubalit® 708 Alumina, 96%
Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is ..
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 600 °C
4.06 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C373
CeramTec Rubalit® 708S Alumina, 96%
Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste..
CTE, linear 7.30 µm/m-°C

@Temperature 25.0 - 500 °C
4.06 µin/in-°F

@Temperature 77.0 - 932 °F
ASTM-C372
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate
This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 600 °C
4.06 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C372
CeramTec CeramCool® Rubalit® 708 Alumina, 96%
CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit..
CTE, linear 7.30 µm/m-°C

@Temperature 20.0 - 600 °C
4.06 µin/in-°F

@Temperature 68.0 - 1110 °F
DIN 51045
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance)
Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn..
Copyright © lookpolymers.com All Rights Reserved