Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 30.0 °C |
4.06 µin/in-°F @Temperature 68.0 - 86.0 °F |
X-Direction |
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 500 °C |
4.06 µin/in-°F @Temperature 68.0 - 932 °F |
|
Misumi Alumina 96 Aluminum Oxide, Al2O3 Information provided by MISUMI Corporation. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG42 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott NG5 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG1, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 7.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BALF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BASF64 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LASF41 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-PSK3 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SK14 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SK16 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott P-LASF47 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 300 °C |
4.06 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott NG3 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG1, NG4, NG5, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 7.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-KZFS4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.06 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-LAF7 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 400 °C |
4.06 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 600 °C |
4.06 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C372 |
CeramTec Rubalit® 708 Alumina, 96% Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is .. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 600 °C |
4.06 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 25.0 - 500 °C |
4.06 µin/in-°F @Temperature 77.0 - 932 °F |
ASTM-C372 |
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 600 °C |
4.06 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C372 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
CTE, linear | 7.30 µm/m-°C @Temperature 20.0 - 600 °C |
4.06 µin/in-°F @Temperature 68.0 - 1110 °F |
DIN 51045 |
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance) Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn.. |