Schott BG42 Band Pass Filter

Category Ceramic , Glass , Filter , Optical
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott BG42 Band Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
Physical Properties Metric English Comments
Density 2.69 g/cc
0.0972 lb/in³
Thermal Properties Metric English Comments
CTE, linear 7.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.06 µin/in-°F

@Temperature -22.0 - 158 °F
8.70 µm/m-°C

@Temperature 20.0 - 300 °C
4.83 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 477 °C
891 °F
Optical Properties Metric English Comments
Refractive Index 1.54

@Wavelength 587.6 nm
1.54

@Wavelength 587.6 nm
He
1.55

@Wavelength 404.7 nm
1.55

@Wavelength 404.7 nm
Hg
Transmission, Visible <= 10 %

@Wavelength 660 - 700 nm
<= 10 %

@Wavelength 660 - 700 nm
84 %

@Wavelength 500 - 530 nm
84 %

@Wavelength 500 - 530 nm
Internal transmittance of 93% from 510-530 nm
IR Transmittance 81 %

@Wavelength 2400 nm
81 %

@Wavelength 2400 nm
Internal transmittance of 89% at 2400 nm.
UV Transmittance <= 0.60 %

@Wavelength 200 - 310 nm
<= 0.60 %

@Wavelength 200 - 310 nm
62 %

@Wavelength 390 nm
62 %

@Wavelength 390 nm
Internal transmittance of 68% at 390 nm
Reflection Coefficient, Visible (0-1) 0.91
0.91
Chemical Properties Metric English Comments
Acid Class, SR 2
2
Alkali Class, AR 2
2
Stain Resistance Class, FR 0.0
0.0