CeramTec Rubalit® 708 Alumina, 96%

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer CeramTec North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CeramTec Rubalit® 708 Alumina, 96%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is also used for precision wire-wound resistors.
Physical Properties Metric English Comments
Density 3.75 g/cc
0.135 lb/in³
Water Absorption 0.00 %
0.00 %
ASTM-C373
Mechanical Properties Metric English Comments
Hardness, Rockwell 45 N 78
78
ASTM-E18
Flexural Strength 420 MPa
60900 psi
Bending Strength; ASTM-F417
Thermal Properties Metric English Comments
CTE, linear 4.40 µm/m-°C

@Temperature 20.0 - 100 °C
2.44 µin/in-°F

@Temperature 68.0 - 212 °F
ASTM-C372
6.30 µm/m-°C

@Temperature 20.0 - 300 °C
3.50 µin/in-°F

@Temperature 68.0 - 572 °F
ASTM-C372
7.30 µm/m-°C

@Temperature 20.0 - 600 °C
4.06 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C372
8.00 µm/m-°C

@Temperature 20.0 - 1000 °C
4.44 µin/in-°F

@Temperature 68.0 - 1830 °F
ASTM-C372
Thermal Conductivity 24.0 W/m-K
167 BTU-in/hr-ft²-°F
ASTM-C408
Maximum Service Temperature, Air 1400 °C
2550 °F
Component Elements Properties Metric English Comments
Al2O3 96 %
96 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm

@Temperature 600 °C
1.00e+8 ohm-cm

@Temperature 1110 °F
ASTM-D1829
1.00e+11 ohm-cm

@Temperature 400 °C
1.00e+11 ohm-cm

@Temperature 752 °F
ASTM-D1829
1.00e+12 ohm-cm

@Temperature 200 °C
1.00e+12 ohm-cm

@Temperature 392 °F
ASTM-D257
Dielectric Strength >= 10.0 kV/mm
>= 254 kV/in
ASTM-D149
Descriptive Properties Value Comments
Color White
Ra = Arithmetic Mean Roughness Value (µm) 0.25-0.35
Te Value (°C) 900