Material Notes:
Information Provided by SCHOTT North America, Inc.
Physical Properties Metric English Comments
Density 3.58 g/cc
0.129 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 600
600
.1/20
Modulus of Elasticity 89.0 GPa
12900 ksi
Poissons Ratio 0.264
0.264
Shear Modulus 35.0 GPa
5080 ksi
calculated
Thermal Properties Metric English Comments
CTE, linear 6.30 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.50 µin/in-°F

@Temperature -22.0 - 158 °F
7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.578 J/g-°C
0.138 BTU/lb-°F
Thermal Conductivity 0.818 W/m-K
5.68 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 636 °C
1180 °F
Optical Properties Metric English Comments
Refractive Index 1.62041

@Wavelength 587.6 nm
1.62041

@Wavelength 587.6 nm
n<sub>d</sub>
1.62286

@Wavelength 546.1 nm
1.62286

@Wavelength 546.1 nm
n<sub>e</sub>
Transmission, Visible 97.1 %

@Thickness 10.0 mm,
Wavelength 380 nm
97.1 %

@Thickness 0.394 in,
Wavelength 380 nm
99 %

@Thickness 10.0 mm,
Wavelength 405 nm
99 %

@Thickness 0.394 in,
Wavelength 405 nm
99.4 %

@Thickness 10.0 mm,
Wavelength 460 nm
99.4 %

@Thickness 0.394 in,
Wavelength 460 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 580 nm
99.8 %

@Thickness 0.394 in,
Wavelength 580 nm
99.8 %

@Thickness 10.0 mm,
Wavelength 700 nm
99.8 %

@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance 58.3 %

@Thickness 10.0 mm,
Wavelength 2500 nm
58.3 %

@Thickness 0.394 in,
Wavelength 2500 nm
98.9 %

@Thickness 10.0 mm,
Wavelength 1530 nm
98.9 %

@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance 1.0 %

@Thickness 10.0 mm,
Wavelength 290 nm
1.0 %

@Thickness 0.394 in,
Wavelength 290 nm
6.3 %

@Thickness 10.0 mm,
Wavelength 300 nm
6.3 %

@Thickness 0.394 in,
Wavelength 300 nm
69.3 %

@Thickness 10.0 mm,
Wavelength 334 nm
69.3 %

@Thickness 0.394 in,
Wavelength 334 nm
95.4 %

@Thickness 10.0 mm,
Wavelength 370 nm
95.4 %

@Thickness 0.394 in,
Wavelength 370 nm
Chemical Properties Metric English Comments
Acid Class, SR 53.3
53.3
Alkali Class, AR 3.3
3.3
Stain Resistance Class, FR 4.0
4.0
Descriptive Properties Value Comments
B 1
Climatic Resistance Test CR 4
HG 4
K (10-6mm2/N) 1.9
Phosphate Resistance PR 3.2
T1013.0 (°C) 633
T107.6 (°C) 750