Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schott NG5 Neutral Density Filter

Category Ceramic , Glass , Filter , Optical
Manufacturer Schott Glas Mainz
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott NG5 Neutral Density Filter.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG1, NG9, NG10, NG11, NG 12
Physical Properties Metric English Comments
Density 2.43 g/cc
0.0878 lb/in³
Thermal Properties Metric English Comments
CTE, linear 6.60 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.67 µin/in-°F

@Temperature -22.0 - 158 °F
7.30 µm/m-°C

@Temperature 20.0 - 300 °C
4.06 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 474 °C
885 °F
Optical Properties Metric English Comments
Refractive Index 1.50

@Wavelength 587.6 nm
1.50

@Wavelength 587.6 nm
He
Transmission, Visible 51 - 55 %

@Wavelength 400 - 700 nm
51 - 55 %

@Wavelength 400 - 700 nm
Internal transmittance of 55-60% from 400-700 nm.
IR Transmittance 64 %

@Wavelength 2500 - 2600 nm
64 %

@Wavelength 2500 - 2600 nm
Internal transmittance of 70% at 2500-2600 nm.
UV Transmittance <= 1.0 %

@Wavelength 200 - 330 nm
<= 1.0 %

@Wavelength 200 - 330 nm
46 %

@Wavelength 390 nm
46 %

@Wavelength 390 nm
Internal transmittance of 50% at 390 nm
Reflection Coefficient, Visible (0-1) 0.92
0.92
Chemical Properties Metric English Comments
Acid Class, SR 3.2
3.2
Alkali Class, AR 2
2
Stain Resistance Class, FR 1
1
Users viewing this material also viewed the following: