Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 110 - 140 µm/m-°C | 61.1 - 77.8 µin/in-°F | Average value: 118 µm/m-°C Grade Count:19 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
CTE, linear, Transverse to Flow | 51.0 - 140 µm/m-°C | 28.3 - 77.8 µin/in-°F | Average value: 87.9 µm/m-°C Grade Count:63 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
CTE, linear, Transverse to Flow | 122 - 140 µm/m-°C | 67.8 - 77.8 µin/in-°F | Average value: 132 µm/m-°C Grade Count:8 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
CTE, linear, Transverse to Flow | 96.0 - 140 µm/m-°C | 53.3 - 77.8 µin/in-°F | Average value: 116 µm/m-°C Grade Count:4 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear, Transverse to Flow | 110 - 140 µm/m-°C | 61.1 - 77.8 µin/in-°F | Average value: 125 µm/m-°C Grade Count:10 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |