Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® 500SC NC010 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® 500SC NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone Lubricated Medium Viscosity Acetal Homopolymer Concentrate Developed for Enhancing LubricityInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 66.0 MPa
9570 psi
ISO 527-1/-2
Elongation at Break 40 %
40 %
Nominal; ISO 527-1/-2
Elongation at Yield 21 %
21 %
ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
ISO 527-1/-2
Flexural Strength 75.0 MPa

@Strain 3.50 %
10900 psi

@Strain 3.50 %
ISO 178
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Charpy Impact Unnotched 27.0 J/cm²
128 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.850 J/cm²
4.04 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
100 µm/m-°C

@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
61.1 µin/in-°F
ISO 11359-1/-2
110 µm/m-°C

@Temperature -40.0 - 23.0 °C
61.1 µin/in-°F

@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code >POM-S20<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM-S20
ISO 1043
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved