Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics ULTEM CRS5201 PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM CRS5201 PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.
Physical Properties Metric English Comments
Specific Gravity 1.42 g/cc
1.42 g/cc
ASTM D792
Melt Flow 2.3 g/10 min

@Load 6.60 kg,
Temperature 337 °C
2.3 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 131 MPa
19000 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 6.89 GPa
999 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 213 MPa
30900 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 6.89 GPa
999 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
4.80 J/cm

@Thickness 3.20 mm
8.99 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 218 °C

@Thickness 6.40 mm
424 °F

@Thickness 0.252 in
unannealed; ASTM D648
Glass Transition Temp, Tg 225 °C
437 °F
UL RTI, Electrical 105 °C
221 °F
UL 746B
UL RTI, Mechanical with Impact 105 °C
221 °F
UL 746B
UL RTI, Mechanical without Impact 105 °C
221 °F
UL 746B
Flammability, UL94 V-0

@Thickness 1.47 mm
V-0

@Thickness 0.0579 in
UL 94
5VA

@Thickness 1.47 mm
5VA

@Thickness 0.0579 in
UL 94
Electrical Properties Metric English Comments
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
Comparative Tracking Index 100 - 175 V
100 - 175 V
UL 746A
Hot Wire Ignition, HWI 30 - 60 sec
30 - 60 sec
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
0.00 - 15 arcs
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/min
>= 5.91 in/min
UL 746A