Material Notes:
Polyether Sulfone Resin-Medium Viscosity, unreinforced standard grade for Easy Injection Molding.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 88.0 MPa
12800 psi
50 mm/min; ASTM D638
Elongation at Break 6.0 %
6.0 %
50 mm/min; ASTM D638
Tensile Modulus 2.60 GPa
377 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 130 MPa
18900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.850 J/cm

@Temperature 23.0 °C
1.59 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 195 °C

@Thickness 3.20 mm
383 °F

@Thickness 0.126 in
unannealed; ASTM D648
Glass Transition Temp, Tg 225 °C
437 °F
ASTM D3482