Thermal Properties Metric English Comments
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman Aqua 20837 PET  (discontinued **)
Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 15041 PET  (discontinued **)
Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 7352 PET  (discontinued **)
VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 9663 PET  (discontinued **)
VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 9921 PET Film  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 9921 PET Injection Molded  (discontinued **)
VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman BD445 PET  (discontinued **)
Voridian Polymer BD445 is primarily targeted for the soft drink and water markets, it is also suitable for use in other beverage containers as well as food and on-food-related applications. This pol..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman CA12 PET  (discontinued **)
Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman CB12 PET  (discontinued **)
Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
Americas Styrenics Styron® 6010 High Impact Polystyrene  (discontinued **)
STYRON® 6010 resin is a high impact polystyrene grade with a proprietary ignition resistance additive package to achieve a UL 94 V-0 rating. It offers high heat resistance, high modulus, good impac..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
Micropol Isoplas P381 Crosslinkable Polyethylene
Information provided by Micropol Limited
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
ASTM C351
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE)
POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
ASTM C351
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
ASTM C351
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
ASTM C351
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
Styron Magnumâ„¢ 4455 ABS
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
DSC
Eastman Eastar A150 Copolyester, Film
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
of Liquid
BASF Isobutyl Acrylate
Formula: C7H12O2CAS: 106-63-8Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: Isobutyl acrylate forms homopolymers and copolymers. Copol..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
DSC
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal..
Specific Heat Capacity 1.90 - 2.30 J/g-°C

@Temperature 100 - 175 °C
0.454 - 0.550 BTU/lb-°F

@Temperature 212 - 347 °F
Average value: 2.10 J/g-°C Grade Count:1
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 5214A PET  (discontinued **)
Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 9921W PET Film  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Specific Heat Capacity 1.90 J/g-°C

@Temperature 200 °C
0.454 BTU/lb-°F

@Temperature 392 °F
ASTM E1269
Eastman 9921W PET Injection Molded  (discontinued **)
Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters ..
Specific Heat Capacity 1.90 - 2.30 J/g-°C

@Temperature 100 - 175 °C
0.454 - 0.550 BTU/lb-°F

@Temperature 212 - 347 °F
Average value: 2.10 J/g-°C Grade Count:3