Polymer Property : Specific Heat Capacity = 0.550 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.84 - 2.30 J/g-°C
0.440 - 0.550 BTU/lb-°F
Average value: 1.87 J/g-°C Grade Count:8
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Specific Heat Capacity 1.90 - 2.30 J/g-°C

@Temperature 100 - 175 °C
0.454 - 0.550 BTU/lb-°F

@Temperature 212 - 347 °F
Average value: 2.10 J/g-°C Grade Count:1
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Specific Heat Capacity 1.90 - 2.30 J/g-°C

@Temperature 100 - 175 °C
0.454 - 0.550 BTU/lb-°F

@Temperature 212 - 347 °F
Average value: 2.10 J/g-°C Grade Count:3
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..