Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.84 - 2.30 J/g-°C | 0.440 - 0.550 BTU/lb-°F | Average value: 1.87 J/g-°C Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Specific Heat Capacity | 1.90 - 2.30 J/g-°C @Temperature 100 - 175 °C |
0.454 - 0.550 BTU/lb-°F @Temperature 212 - 347 °F |
Average value: 2.10 J/g-°C Grade Count:1 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Specific Heat Capacity | 1.90 - 2.30 J/g-°C @Temperature 100 - 175 °C |
0.454 - 0.550 BTU/lb-°F @Temperature 212 - 347 °F |
Average value: 2.10 J/g-°C Grade Count:3 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |