Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D792
Melt Flow 1.75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 250 %
250 %
Modulus of Elasticity 1.10 GPa

@Temperature 20.0 °C
160 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
Specific Heat Capacity 1.90 J/g-°C
0.454 BTU/lb-°F
Thermal Conductivity 0.431 W/m-K
2.99 BTU-in/hr-ft²-°F
Vicat Softening Point 126 °C
259 °F
ASTM D1525