Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® PA6/6 Impact Modified 4120 HS Nylon 6/6; MoS2 lube

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Nylene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® PA6/6 Impact Modified 4120 HS Nylon 6/6; MoS2 lube.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
ASTM D790
Izod Impact, Notched 7.88 J/cm
14.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C
147 °F
ASTM D648