Ashley Polymers Ashlene® 528L-30LG Nylon 66, 30% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 528L-30LG Nylon 66, 30% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Long glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.90 %
0.90 %
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 191 MPa
27700 psi
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Flexural Strength 242 MPa
35100 psi
ASTM D790
Flexural Modulus 8.70 GPa
1260 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 251 °C
484 °F
ASTM D648