Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A UV Stabilized 20% glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Modulus 4.80 GPa
696 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 249 °C
480 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
469 °F
ASTM D648