Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A high impact nylon with 14% glass.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Typical value for 13% glass-filled nylon 66
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 94.0 MPa
13600 psi
ATSM D638
Elongation at Break 5.7 %
5.7 %
ASTM D638
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm
2.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Users viewing this material also viewed the following: