Material Notes:
Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Flexural Modulus 1.71 GPa
248 ksi
ASTM D790
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648