Polymer Property : Melting Point = 460 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 232 - 238 °C
450 - 460 °F
Indium Corp. Indalloy® 131 97Sn/3Sb Lead-Free Solder Alloy
Information provided by the manufacturer, Indium Corporation.
Melting Point 183 - 238 °C
361 - 460 °F
Johnson Matthey JM4060 Soft Solder/Flux
General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi..
Melting Point 183 - 238 °C
361 - 460 °F
Indium Corp. Indalloy 130 Tin-Lead Solder Alloy
Inexpensive utility solderInformation Provided by Indium Corporation
Melting Point 234 - 238 °C
453 - 460 °F
SK Chemicals SKYPET® BR8040 Low Content CHDM Modified Copolyester Resin
Description: SKYPET-BR8040 is a low content CHDM modified copolyester resin for large sized-mineral water bottles and extruded sheet. SKYPET-BR8040 has sufficiently low crystallization rate for lar..
Melting Point 183 - 238 °C
361 - 460 °F
Williams Advanced Alloys WS238 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 232 - 238 °C
450 - 460 °F
Williams Advanced Alloys WS238A Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® 6MPB Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® 6MPY Plasticized Nylon 6
A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® 6PA-Blue Nylon 6
NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® 6PA-MoS2 Nylon 6
NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade
NYCAST® 6 PA-Natural along with NYCAST® 6 PA-Blue are two of the most widely used cast nylons in industry. Nylons have replaced bronze, brass, steel, and aluminum in various mechanical applicatio..
Melting Point 227 - 238 °C
440 - 460 °F
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6
NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Melting Point 227 - 238 °C
440 - 460 °F
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6
NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® Nyloil® Lubricated Nylon
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than ..
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Cast Nylons Nycast® XHA Heat Stabilized Nylon 6
Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Dat..
Melting Point 190 - 238 °C
374 - 460 °F
Average value: 219 °C Grade Count:60
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..