Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 226 °C | 439 °F | |
Samyang Tribit® 1500 Polybutylene Terephthalate Characteristics:Medium viscosityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samy.. |
|||
Melting Point | 226 °C | 439 °F | |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Melting Point | 226 °C | 439 °F | |
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Melting Point | 226 °C | 439 °F | |
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Melting Point | 226 °C | 439 °F | |
Samyang Tribit® 1500GN30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Melting Point | 226 °C | 439 °F | |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Melting Point | <= 226 °C | <= 439 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Melting Point | <= 226 °C | <= 439 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin Product Description: LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a .. |
|||
Melting Point | <= 226 °C | <= 439 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 160AT Low Density Polyethylene Resin Product Description: LD 160 series are LDPE grades, which offer good draw down and optical properties.Availability: Africa & Middle East, Asia Pacific, Latin America, North America and South America.. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® 6MPB Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPB is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® 6MPY Plasticized Nylon 6 A plasticized Type 6 material, NYCAST® 6MPY is formulated for use as pile driver caps or cushion pads. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values prese.. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® 6PA-Blue Nylon 6 NYCAST® 6 PA-Blue along with NYCAST® 6 PA-Natural have replaced bronze, brass, steel, and aluminum in various mechanical applications.Data provided by the manufacturer, Cast Nylons Limited.The dat.. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® 6PA-MoS2 Nylon 6 NYCAST® 6PA-MoS2 is a molybdenum disulphide filled Type 6 cast nylon. Finely divided MoS2 particles are suspended in the melt during polymerization. This gives the NYCAST® 6PA-MoS2 products improv.. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® 6PA-Natural Nylon 6, Food Grade NYCAST® 6 PA-Natural along with NYCAST® 6 PA-Blue are two of the most widely used cast nylons in industry. Nylons have replaced bronze, brass, steel, and aluminum in various mechanical applicatio.. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
Melting Point | 226 - 238 °C | 439 - 460 °F | ASTM D789 |
Cast Nylons Nycast® XHA Heat Stabilized Nylon 6 Heat stabilized Cast Nylon 6 adds up to 20 degrees F higher continuous operation temperature for those applications that require additional temperature resistance beyond the standard resistance. Dat.. |