Material Notes:
NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than unlubricated or MoS2 dry lubricated cast nylons. Lubrication results in 25% lower coefficient of friction. NYCAST® NYLOILS exhibit more dimensional stability due to reduced moisture absorption. Internal lubricant provides for faster and easier machining than other nylons. Data provided by the manufacturer, Cast Nylons Limited.The data below are average values presented for comparison purposes. Actual property values may differ.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs; ASTM D570
Water Absorption at Saturation 2.5 %
2.5 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Elongation at Break 35 - 45 %
35 - 45 %
ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Flexural Yield Strength 109 MPa
15800 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Compressive Yield Strength 95.0 MPa
13800 psi
10% Offset; ASTM D695
Compressive Modulus 2.40 GPa
348 ksi
ASTM D695
Shear Strength 59.0 MPa
8560 psi
ASTM D732
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Tensile Impact Strength 72.0 kJ/m²
34.3 ft-lb/in²
ASTM D1822
Coefficient of Friction, Dynamic 0.12
0.12
Coefficient of Friction, Static 0.20
0.20
K (wear) Factor 8.06 x 10-8 mm³/N-M
4.00 x 10-10 in³-min/ft-lb-hr
unlubricated thrust washer machine @ 10 fpm and 250 psi
Limiting Pressure Velocity 0.560 MPa-m/sec
16000 psi-ft/min
at 1.27 m/s
1.33 MPa-m/sec
38000 psi-ft/min
at 0.127 m/s
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 226 - 238 °C
439 - 460 °F
ASTM D789
Maximum Service Temperature, Air 110 °C
230 °F
Continuous service
166 °C
331 °F
Intermittent service
Deflection Temperature at 0.46 MPa (66 psi) 204 - 221 °C
399 - 430 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 166 - 204 °C
331 - 399 °F
ASTM D648