Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 210 - 212 °C | 410 - 414 °F | Average value: 211 °C Grade Count:14 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Melting Point | 183 - 212 °C | 361 - 414 °F | |
Indium Corp. Indalloy 116 Tin-Lead Solder Alloy General purpose solderInformation Provided by Indium Corporation |
|||
Melting Point | 183 - 212 °C | 361 - 414 °F | |
Williams Advanced Alloys WS212 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 210 - 212 °C | 410 - 414 °F | |
Daikin NEOFLON M-300H PCTFE Granular Molding Powder NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Granular powders.Processing Methods: Compression molding, extrusion.Uses: Sheets, rods, tubing.Information provided by.. |
|||
Melting Point | 210 - 212 °C | 410 - 414 °F | |
Daikin NEOFLON M-300P PCTFE Pellets NEOFLON PCTFE M-300 series is used for general purpose applications.Description:Pellets.Processing Methods: Extrusion.Uses: Rods, small parts.Information provided by Daikin Industries. |
|||
Melting Point | 210 - 212 °C | 410 - 414 °F | |
Daikin NEOFLON M-400H PCTFE Granular Molding Powder NEOFLON PCTFE M-400 series is a high molecular weight type material which is suitable for applications requiring mechanical toughness and stress crack resistance.Description:Granular powders.Process.. |