Indium Corp. Indalloy 116 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 116 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose solderInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.87 g/cc
0.320 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 14
14
Tensile Strength at Break 41.4 MPa
6000 psi
Elongation at Break 35 %
35 %
Shear Strength 35.9 MPa
5200 psi
Thermal Properties Metric English Comments
CTE, linear 23.0 µm/m-°C

@Temperature 20.0 °C
12.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 48.0 W/m-K

@Temperature 85.0 °C
333 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 183 - 212 °C
361 - 414 °F
Solidus 183 °C
361 °F
Liquidus 212 °C
414 °F
Component Elements Properties Metric English Comments
Lead, Pb 50 %
50 %
Tin, Sn 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000158 ohm-cm
0.0000158 ohm-cm