Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTROPEEK Polyetheretherketone

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROPEEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROPEEK Polyetheretherketone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This plastic has high temperature resistance, good chemical resistance, and good mechanical characteristics. Its has good sliding friction properties and is suitable for use with foodstuffs or medical equipment.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.20 %
0.20 %
in normal climate 23°C/50%RH; ISO 62
Water Absorption at Saturation 0.45 %
0.45 %
in water at 23°C; ISO 62
Mechanical Properties Metric English Comments
Hardness, Rockwell M 105

@Thickness 10.0 mm
105

@Thickness 0.394 in
ISO 2039-2
Ball Indentation Hardness 230 MPa
33400 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 110 MPa
16000 psi
v = 50 mm/min; ISO 527-2
Elongation at Break 20 %
20 %
ISO 527-2
Tensile Modulus 4.40 GPa
638 ksi
ISO 527-2
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
ISO 11359
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
Melting Point 340 °C
644 °F
10K/min; ISO 3146
Maximum Service Temperature, Air 250 °C
482 °F
Long Term
310 °C
590 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-2
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.2

@Frequency 100 Hz
3.2

@Frequency 100 Hz
IEC 60250
3.6

@Frequency 1e+6 Hz
3.6

@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm
610 kV/in
in transformer oil; IEC 60243-1
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
IEC 60250
0.0020

@Frequency 1e+6 Hz
0.0020

@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 V
150 V
IEC 60112
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved