Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids, and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing, and other industrial uses. The resin is also available as KetaSpire KT-820 NT in a natural-color pellet form for injection molding and extrusion.Injection Notes: Back Pressure: minimumInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Particle Mesh Size >= 100 Mesh
>= 100 Mesh
0% Retained on 100 mesh sieve
>= 140 Mesh
>= 140 Mesh
< 2.0% Retained on 140 mesh sieve
Mechanical Properties Metric English Comments
Tensile Strength 96.5 MPa
14000 psi
ASTM D638
Elongation at Break 20 - 30 %
20 - 30 %
Crystallized; ASTM D638
>= 60 %
>= 60 %
Quenched; ASTM D638
Elongation at Yield 5.2 %
5.2 %
ASTM D638
Tensile Modulus 3.65 GPa
529 ksi
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
23.9 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Melting Point 340 °C
644 °F
ASTM D3417
Deflection Temperature at 1.8 MPa (264 psi) 162 °C
324 °F
Unannealed; ASTM D648
Glass Transition Temp, Tg 150 °C
302 °F
ASTM D3417
Descriptive Properties Value Comments
Appearance Natural Color
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Ductile
Fatigue Resistant
Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
Good Impact Resistance
High Heat Resistance
Forms Powder
Generic PEEK
Processing Method Compression Molding
Uses Electrical/Electronic Applications
Industrial Applications
Oil/Gas Applications
Copyright © lookpolymers.com All Rights Reserved