Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.Recommended Applications. 3860X is recommended for nonwoven fiber applications.FDA. 3860X complies with all applicable FDA regulations for food contact applications.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 100 g/10 min
100 g/10 min
ASTM D1238, L
Mechanical Properties Metric English Comments
Tensile Modulus 1.655 GPa
240.0 ksi
ASTM D638
Flexural Modulus 1.517 GPa
220.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC