Material Notes:
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional hardness and strength even without any addition of reinforced structure material. It is resistant to alkalis and hot water. It is resistant to organic solvents which are commonly used, to petroleum products and to many of the mineral oils.PROPERTIES OF POLIPOM®:Dimensional StabilityHigh Resistance To Loads and StrokesExcellent Resistance To CorrosionHigh Mechanical Strength and Non-TwistingHigh ElasticityBearing Property at Environments Without OilHigh Electrical Insulation PropertyLow Absorption Resistance To Heat(-50°C - +110°C / short period 150°C)GENERAL USAGE AREAS OF POLIPOM®: As per its above mentioned technical properties, POLIPOM® is most commonly used in the production of machine molding parts at all sectors; gears, bearings of rolling mills and bearings exposed to extreme loads, conveyor systems, pins, unlimited screws, pistons, pivots and areas like these. Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.
Physical Properties Metric English Comments
Specific Gravity 1.41 - 1.43 g/cc
1.41 - 1.43 g/cc
ISO.1183 DN.53479
Water Absorption 0.50 %
0.50 %
ISO.62 DN.53495
Mechanical Properties Metric English Comments
Hardness, Rockwell M 78 - 86
78 - 86
ISO.2039-2
Hardness, Shore D 75
75
DN.53505
Ball Indentation Hardness 140 - 155 MPa
20300 - 22500 psi
ISO.2039-2
Tensile Strength at Break 70.0 MPa
10200 psi
ISO.527 DN.53455
Tensile Strength, Yield 62.0 - 71.0 MPa
8990 - 10300 psi
ISO.527 DN.53455
Elongation at Break 20 - 75 %
20 - 75 %
ISO.527 DN.53455
Elongation at Yield 8.0 - 10 %
8.0 - 10 %
ISO.527 DN.53455
Modulus of Elasticity >= 2.70 GPa
>= 392 ksi
ISO.178 DN.53452
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO.179 DN.53453
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
DN.53752
Melting Point 165 - 175 °C
329 - 347 °F
Maximum Service Temperature, Air 100 °C
212 °F
ISO.75 DN.53461
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ISO.167 DN.53482
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
ISO.167 DN.53482
Dielectric Strength >= 50.0 kV/mm
>= 1270 kV/in
ISO.243 DN.53481