Thermal Properties Metric English Comments
Melting Point 165 - 175 °C
329 - 347 °F
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..
Melting Point 165 - 175 °C
329 - 347 °F
Polimersan Plastics POLIPOM® (POM)
POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional..
Melting Point 165 - 175 °C
329 - 347 °F
MQSA 111
Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e..
Melting Point 171 - 175 °C
340 - 347 °F
ASTM D3418
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Melting Point 170 - 175 °C
338 - 347 °F
ASTM D3418
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers.
Melting Point 170 - 175 °C
338 - 347 °F
ASTM D3418
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Melting Point 160 - 175 °C
320 - 347 °F
Huntsman/TMA
Huntsman IROGRAN® A 78 E 4588 Polyester-Based TPU-High Performance Grade
High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman
Melting Point 160 - 175 °C
320 - 347 °F
Huntsman/TMA
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
Melting Point 165 - 175 °C
329 - 347 °F
Huntsman/TMA
Huntsman IROGRAN® A 85 D 5001 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
Melting Point 165 - 175 °C
329 - 347 °F
Indium Corp. Indalloy® 204 In-Pb Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Melting Point 165 - 175 °C
329 - 347 °F
Sheath Melt Point; LCL-PR29
Intercontinental Polymers 1631 Bicomponent Polyester/PET Fiber Type - 4 Denier X 2 Inches
Semi-crystalline low melt polyester sheath/PET core. Luster: Semi-Dull. Finish: HydrophilicApplications of bicomponent polyester fiber: Absorbent products, FDA-compliant products, non-wovens, fi..
Melting Point 155 - 175 °C
311 - 347 °F
Huntsman/TMA
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether
Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext..
Melting Point 122 - 175 °C
252 - 347 °F
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester
Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi..
Melting Point 165 - 175 °C
329 - 347 °F
MQSA 111
Lubrizol Advanced Materials PEARLCOAT® 165K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 165K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and very good hydrolysis resistance. PE..
Melting Point 170 - 175 °C
338 - 347 °F
ASTM D789
Lucent Polymers POM-900P Acetal Homopolymer, Easy Flow, Injection Grade
Add "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Melting Point 170 - 175 °C
338 - 347 °F
DSC
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF)
Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope..
Melting Point 171 - 175 °C
340 - 347 °F
DSC
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition..
Melting Point 170 - 175 °C
338 - 347 °F
DSC
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D..
Melting Point 170 - 175 °C
338 - 347 °F
DSC
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6..
Melting Point 171 - 175 °C
340 - 347 °F
DSC
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran..
Melting Point 145 - 175 °C
293 - 347 °F
DSC; ASTM D3418
Lubrizol Estane® X-585A-31 Thermoplastic Polyurethane
Type: Estane® X585A-31 is a Shore 95A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizol..
Melting Point 165 - 175 °C
329 - 347 °F
ISO 11357
Polyram PlusTek PD305G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced
30% Glass-fiber reinforced Nylon 12 for injection molding applications.Information provided by Polyram.
Melting Point 165 - 175 °C
329 - 347 °F
Polyram PlusTek RD101 Nylon 12, Injection Molding
Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind.
Melting Point 165 - 175 °C
329 - 347 °F
Polyram PlusTek RD302G6 Nylon 12, 30% Glass Fiber
30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Melting Point 165 - 175 °C
329 - 347 °F
Polyram PlusTek PD100 Nylon 12, Injection Molding
Outstanding polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind.
Melting Point 165 - 175 °C
329 - 347 °F
Polyram PlusTek PD300G6 Nylon 12, 30% Glass Fiber
30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Melting Point 165 - 175 °C
329 - 347 °F
ISO 11357
Polyram PlusTek PD304G6YL55 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced
30% Glass-fiber reinforced Nylon 12 for injection molding applications. UL listed.Information provided by Polyram.
Melting Point 165 - 175 °C
329 - 347 °F
ISO 11357
Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced
30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram.
Melting Point 171 - 175 °C
340 - 347 °F
ASTM D3418
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Melting Point 170 - 175 °C
338 - 347 °F
ASTM D789
Lucent Polymers POM-500 Acetal Homopolymer, General Purpose, Injection Grade