Material Notes:
THV 510ESD is a flexible, fluoroplastic compound composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provides a balance of low temperature processing, low flammability, thermal stability, and melt processability along with electrostatic dissipative properties. IT can be used to prepare molded parts and extruded films, tubes and profiles. It is useful for applications that require electrostatic dissipation, flexibility, low temperature processing, and go chemical resistance.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 1.95 g/cc
1.95 g/cc
ASTM D792
Melt Index of Compound 3.5 - 8.5 g/10 min

@Load 5.00 kg,
Temperature 265 °C
3.5 - 8.5 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Flexural Modulus 0.440 GPa
63.8 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ASTM D4591
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm - 1e+05
1000 ohm-cm - 1e+05
ASTM D257
Descriptive Properties Value Comments
Form Pellets